| hdd-1 | hdd-2 | hdd-3 | hdd-4 | hdd-5 |
化学成分(%) chemical composition | sio2≥ | 98 | 98 | 96 | 96 | 90 |
al2o3≤ | 0.7 | 0.6 | 0.6 | 0.5 | 0.4 |
fe2o3≤ | 0.5 | 0.5 | 0.4 | 0.4 | 0.8 |
冷态耐压强度(mpa) cold crushing strength | 1300℃×3h after firing at | 15 | 15 | 10 | 10 | 25 |
显气孔率(% apparent porosity | 1300℃×3h after firing at | 26 | 26 | 25 | 25 | 23 |
烧后线变化率(%) linear changing after burnt | 1300℃×3h after firing at | 0~+1.6 | 0~+1.2 | 0~+1.0 |
体积密度(g/cm3) bulk density | 1300℃×3h after firing at | 2.0 | 2.0 | 2.1 | 2.1 | 2.2 |
耐火度(℃)refractoriness | 1750 | 1750 | 1750 | 1750 | — |
最大集料粒度(mm) max. grain size of aggregate | 5 | 4.5 | 4.5 | 4.2 | 4.2 |
施工用量(kg/m3)amount for construction | 2300 | 2300 | 2300 | 2400 | 2400 |
施工方式mathod of construction | 振动或捣打jolt or ramming |
应用 application | 紫铜.黄铜 青铜 copper brassbronze | 紫铜.黄铜copper brass | 白铜cupronickel | 钢铁 steel | 铝 aluminium |
有色金属熔炼炉melting furance for nonferrous metals 适用于100kw以下感应电炉最佳 be the same with 100kw hereinafter inductance furnace |
特点characteristic | 价廉保温节电不沾渣快速干燥化学结合耐侵蚀 cost down thernalinsulation economy electricity nostickresidue fast drying chemicalbonded corrosion resistance |
| | | | | | | | | |