碳化硅砖的各项技术指标
项目 |
氧化物结合碳化硅转 oxide bond sic brick |
刚玉碳化硅砖 cor-silicon carbide brick |
莫来石碳化硅砖 mullite-sic brick |
硅莫砖 |
sic% |
≥90 |
≥70 |
≥65 |
≥20 |
al2o3% |
- |
- |
≥20 |
≥65 |
体积密度g/cm3 bulk density |
≥2.5 |
≥2.6 |
≥2.3 |
≥2.55 |
显气孔率% apparent porosity |
≤17 |
≤22 |
≤20 |
≤19 |
常温耐压强度mpa cold crushing strength |
≥100 |
≥100 |
≥80 |
≥80 |
荷重软化开始温度℃(0.2mpa ,0.6%) refractoriness under load |
≥1650 |
≥1700 |
≥1600 |
≥1600 |
导热系数(1000℃),w/(m·k) thermal conductivity |
10-15 |
6 |
- |
- |